capricorn-xs-series-ptfe-bowden-tubing-for-1-75mm-filament
capricorn-xs-series-2capricorn-xs-series-3

Capricorn XS-Tub PTFE 1,75mm

Cod Produs: RRM-4203

lei44.00

Pretul este pentru 50cm!

În stoc

Categorii: ,

Descriere Produs

Tub  PTFE  îmbogățit cu un amestec propriu de aditivi de înaltă performanță. 1,9 mm interior, 4 mm diametru exterior pentru filamente de 1,75 mm.
Aceasta este,  cel mai bun PTFE Bowden pe care îl puteți cumpăra pentru imprimanta 3D

Garantat să fie mereu diametrul potrivit și perfect rotund. Imprimați filamentele flexibile cu usurinta folosint Caprocorn XS

Pretul este pentru 50cm!!, lungimea maxima de livrare pentru o bucata este de 1 metru!!!

Detalii tehnice(furnizate de producator)
Our Premium XS Series Dark Blue Tubing
Additives Blue Color and Secret High Lubricity Additive Mixture
Best For Chunky Filaments YES
Best For Flexible Filaments YES
Can See Through NO
Pulling Friction 0.8
Color Dark Blue
Density (kg/m3) 2300 +/-100
Hardness 60-65
Inner Diameter (mm) 1.90 +/- 0.05
Linear Thermal Expansion at 250 °C 2.2-3.3%
Material Highest Quality Pure Virgin PTFE
Melting Point (°C) up to 340
Outer Diameter 3.95 +/- 0.05
Roundness (ϵ) < 0.1
Stiffness§ Medium High
Thermal Conductivity (W/m-k) 0.25
Wear Rate (gm/s) 0.01
Young’s Modulus (GPa)¥ 0.53
Pulling Friction is calculated as the average force required to pull 1.2 meters of 1.75mm PLA filament through 1 meter of tubing at a constant speed, relative to 1 meter of cheap white reference tubing. Note that although we observed the friction of the TL series to be about the same or even slightly lower than our XS series, it also has a larger internal diameter.
§Other Bowden tubes may vary significantly in stiffness, depending on the material from which they’re made. Our tubing generally tends to be more flexible than most, with the TL being more flexible than XS.
¥Young’s Modulus (YM) is the measure of elasticity of the material. Our XS Series additives give the PTFE a slightly greater YM than the TL Series.
Temperatures were approximated by heating samples of all tubing simultaneously, observing how quickly each one began to deform. Printer failures may happen at significantly lower temperatures.